| 1 | Match the grade to the environment. Consider moisture, cleaning chemicals, salt, and outdoor exposure. | 304 is commonly selected for general corrosion resistance. 201 is often used in less demanding environments. 430 is a magnetic ferritic grade commonly used for indoor applications with moderate corrosion requirements. | For coastal, chloride-rich, or frequently wet service, confirm that the grade is suitable for the specific exposure rather than choosing on price alone. |
| 2 | Verify the grade and material certificate. Do not rely on appearance or a magnet test alone. | Typical ASTM A240 composition ranges include 201: 16–18% chromium and 3.5–5.5% nickel; 304: 18–20% chromium and 8–10.5% nickel; 430: 16–18% chromium and no more than 0.75% nickel. | Request documentation identifying the grade, applicable specification, heat or batch number, and supplied dimensions. Composition limits should be checked against the specified standard and product form. |
| 3 | Choose thickness for the job. Account for loads, forming, welding, support spacing, and fabrication tolerances. | Thin sheet is easier to form but can dent or distort more readily; thicker plate is stiffer and heavier. Common commercial offerings span roughly 0.3 mm to 6 mm, but availability and the sheet-versus-plate cutoff vary by supplier and standard. | Specify thickness in millimetres or inches and state whether the required value is nominal or minimum. Confirm permitted thickness tolerances before ordering. |
| 4 | Specify the surface finish. Finish affects appearance, cleaning, reflectivity, and fabrication. | 2B is a common smooth, moderately reflective mill finish; BA is bright annealed and more reflective; No. 4 has a brushed appearance; No. 1 is a rougher hot-rolled, annealed, and pickled finish. | State the finish code and, for brushed finishes, the desired direction or sample standard. Protective film may be available for some finishes and should be specified if needed. |
| 5 | Confirm width and length. The right cut size can reduce scrap and extra processing. | Common stock widths include approximately 1,000, 1,219, 1,250, and 1,500 mm. Common sheet lengths include approximately 2,000, 2,438, 2,500, and 3,000 mm; actual stock sizes vary by grade, thickness, finish, and market. | Provide the required width and length, quantity, and whether pieces should be supplied as standard sheets or cut to size. Confirm dimensional tolerances and squareness requirements. |
| 6 | Consider magnetism and forming. Magnetic response can affect design or fabrication expectations. | Annealed 304 and 201 are generally austenitic and usually weakly magnetic or nonmagnetic, but cold working can induce some magnetism. 430 is ferritic and magnetic. | If magnetism matters, specify the requirement and discuss testing with the supplier. For deep drawing or tight bends, confirm the grade, temper, thickness, and minimum bend guidance for the intended process. |
| 7 | Check flatness, edges, and delivery protection. Handling condition affects cutting, assembly, and visible surfaces. | Surface condition, flatness, edge condition, and protective packaging can vary between mill-finished and cut-to-size material. Cut edges may require deburring or further finishing. | Record flatness and edge requirements, allowable surface marks, packaging, and inspection criteria in the purchase specification. Inspect dimensions and finish on receipt. |