| Carrier Resin | PE type, compatibility, and suitability for the end-use resin | Choose a carrier compatible with the base polymer and process. LDPE or LLDPE carriers are common in film applications; HDPE carriers may suit some stiffer PE products. Confirm compatibility for blends and multilayer structures. | A well-matched carrier can support consistent dispersion and reduce the risk of gels, weak spots, or processing issues. |
| Colorant or Additive Content | Concentrate loading and the recommended let-down ratio | Concentrations vary widely. White concentrates often use high titanium dioxide loading, while black concentrates use carbon black. Colored and additive concentrates depend on the pigment or active ingredient. Compare the finished-part result at the proposed dosage, not loading alone. | Higher loading does not automatically mean better performance; dispersion, formulation, and dosage determine the result. |
| Recommended Dosage | Let-down range by application and target performance | Request a recommended dosage for the actual product thickness, color target, resin, and process. Establish dosage through trials and record it as a percentage of total feed. | Dosage affects color strength, opacity, additive performance, cost, and sometimes mechanical properties. |
| Melt Flow Rate (MFR) | Test result, test conditions, and relevance to the processing method | Compare MFR values only when the test temperature and load are the same. Polyethylene MFR is commonly reported at 190°C; the load should also be stated. Match flow behavior to the base resin and equipment rather than selecting by number alone. | Large flow differences can affect feeding, mixing, pressure, surface appearance, and uniformity. MFR may be reported using ISO 1133-1 or ASTM D1238. |
| Dispersion | Pigment or additive distribution, agglomerates, specks, and gels | Ask how dispersion is evaluated and request application-relevant samples or test results. Assess finished film, sheet, or molded parts at the intended dosage and screen pack or filtration conditions. | Poor dispersion can cause visible defects, uneven color, inconsistent performance, and screen changes. |
| Color Consistency | Color target, measurement method, and batch-to-batch tolerance | Agree on a physical or digital color standard, sample preparation method, and acceptable color difference. For instrumental comparison, specify the color space and measurement conditions, such as CIELAB and illuminant. | Color readings can vary with substrate, thickness, surface, and measurement setup, so matched test conditions are essential. |
| Opacity or Tint Strength | Coverage, whiteness, blackness, or color strength at the target dosage | Test at the intended part thickness and resin. For white concentrates, compare opacity and appearance; for black or colored concentrates, assess the required shade and strength in the actual product. | A result in a laboratory plaque may not predict coverage or appearance in thin film or a different geometry. |
| Thermal Stability | Processing-temperature range and resistance to discoloration or degradation | Confirm suitability for the full melt-temperature profile and residence time, including expected process variation. Ask for guidance for the specific extrusion, molding, or film process. | Insufficient stability can cause color shift, odor, deposits, or reduced additive effectiveness. |
| Moisture and Volatiles | Moisture specification, packaging condition, and drying guidance | Request the supplier’s stated moisture or volatile limits and test method. Keep bags sealed and follow the handling or drying instructions; do not assume that every PE concentrate requires drying. | Excess moisture or volatiles can contribute to bubbles, surface defects, or processing instability, depending on the formulation and process. |
| Filterability and Screen-Pack Behavior | Pressure build-up, screen life, and compatibility with the production filter | Evaluate under representative throughput, screen mesh, temperature, and dosage. Ask for application-specific filtration data where screen changes are a critical cost or quality factor. | Filterability can affect line uptime and is influenced by dispersion, contamination, and the concentrate formulation. |
| Mechanical-Property Impact | Changes to tensile behavior, impact performance, elongation, or stiffness | Test the finished formulation at the intended dosage against an uncolored or additive-free control. Include the properties that matter to the product specification. | Pigments, additives, and carrier differences can affect finished-part properties, particularly at higher addition levels. |
| Weathering and UV Performance | Outdoor exposure requirement, target service life, and test evidence | For outdoor products, specify the exposure environment and required performance. Compare relevant weathering data and validate the complete formulation, including pigment, stabilizer, base resin, and part thickness. | UV performance depends on the full formulation and use conditions; a general claim or additive loading alone does not establish service life. |
| Regulatory and Food-Contact Status | Intended market, application, restricted substances, and supporting declarations | Request current documentation for the exact grade and intended use. Requirements differ by jurisdiction and conditions of use; examples include applicable EU food-contact rules and relevant U.S. FDA regulations. | Regulatory suitability is application- and market-specific and should be verified for the finished article, not inferred from a generic statement. |
| Odor and Migration | Organoleptic requirements and potential migration restrictions | For sensitive packaging or consumer applications, assess odor and migration using methods appropriate to the intended use and applicable regulations. | These properties can affect consumer acceptance and compliance even when the product’s appearance and processing are satisfactory. |
| Process Compatibility | Suitability for blown film, cast film, pipe, sheet, injection molding, or other processes | Confirm performance on the intended line, including feeding, screw design, mixing, output, and part geometry. Avoid assuming that a grade proven in one process will perform identically in another. | Shear, residence time, cooling, and product thickness differ by process and can change final appearance and performance. |
| Quality Control and Traceability | Batch consistency, certificate of analysis, change control, and lot identification | Agree on the critical-to-quality parameters, test methods, and documentation supplied with each lot. Confirm how formulation or raw-material changes are communicated. | Documented controls make incoming inspection, troubleshooting, and long-term production consistency easier. |
| Total Cost in Use | Dosage, yield, scrap, line efficiency, and delivered cost | Compare cost per kilogram of finished product at the validated dosage. Include color or additive performance, production speed, screen changes, waste, and quality losses. | The lowest price per kilogram of concentrate may not deliver the lowest overall production cost. |